RE: [Histonet] formic acid decal

From:"Elizabeth Chlipala"

Trisha

I have used 20% formic acid made up in distilled water on sheep tibias
and it worked just fine.

Liz

Elizabeth A. Chlipala, BS, HTL(ASCP)QIHC
Manager
Premier Laboratory, LLC
P.O. Box 18592
Boulder, Colorado 80308
Office: (303) 735-5001
Fax: (303) 735-3540
liz@premierlab.com
www.premierlab.com
 
Ship to Address:
Premier Laboratory
University of Colorado
MCDB, Room A3B40
Boulder, Colorado 80309

-----Original Message-----
From: histonet-bounces@lists.utsouthwestern.edu
[mailto:histonet-bounces@lists.utsouthwestern.edu] On Behalf Of Trisha
Emry
Sent: Thursday, June 16, 2005 2:54 PM
To: histo
Subject: [Histonet] formic acid decal

I need to speed up the decal process on some large bone samples.
What is the highest precentage of formic acid that I can use without
damaging the bones?

I am using sodium formate with formic acid now.

Thanks,
Trisha
Seattle


_______________________________________________
Histonet mailing list
Histonet@lists.utsouthwestern.edu
http://lists.utsouthwestern.edu/mailman/listinfo/histonet


_______________________________________________
Histonet mailing list
Histonet@lists.utsouthwestern.edu
http://lists.utsouthwestern.edu/mailman/listinfo/histonet


<< Previous Message | Next Message >>