RE: Stereology on thick sections/technovit 7200

From:rita.russell@syngenta.com

Sorry!!!Yes you're right it is 7100(GMA) we used.

> ----------
> From: 	Linda Durbin[SMTP:Linda.Durbin@ExaktUSA.com]
> Sent: 	12 July 2001 01:20
> To: 	Russell Rita GBAP
> Subject: 	RE: Stereology on thick sections/technovit 7200
> 
>  Rita:
> 
> Are you really using Technovit 7200 or is it 7100 (GMA).  Or maybe
> 9100(MMA).  7200 is very brittle.  If it is 7200 I'd love to know how
> you're
> softening it.
> 
> Thanks in advance.
> 
> Linda Durbin
> 
> 
> -----Original Message-----
> From: rita.russell@syngenta.com
> To: histonet@pathology.swmed.edu
> Sent: 7/11/01 2:15 AM
> Subject: Stereology on thick sections/technovit 7200
> 
> We cut sections of whole rat brains at 30 microns embedded in tecnovit
> 7200
> using a solid tungsten carbide knife. Keep the edge of the knife moist
> but
> not too wet with distilled water, and cut very slowly. Float out on
> distilled wa