RE: H&E on plastic, which plastic? Re: [Histonet] eosinhematoxyli n plastic stain
Are your sections thin, i.e. 5 um versus thick, 50 um? as Myriam
indicated.. Do you remove the plastic BEFORE staining? Please provide some
details
Thanks
At 11:43 PM 12/6/2004, you wrote:
>Hello,
>
>I have been doing H&E on bones embedded in methylmetacrylate, and it worked
>fine! I used hematoxylin after GILL and alcoholic Eosin.
>Tina
Gayle Callis
MT,HT,HTL(ASCP)
Research Histopathology Supervisor
Veterinary Molecular Biology
Montana State University - Bozeman
PO Box 173610
Bozeman MT 59717-3610
406 994-6367 (lab with voice mail)
406 994-4303 (FAX)