Hi Jennifer,
We soak all the glassware to be used for silver solutions in 10% nitric
acid for approx. 30 min. and then rinse well (at least three times) in
distilled water.
Katri
Katri Tuomala
Anatomic Pathology
St.Joseph's Hospital
Hamilton, Ontario, Canada